Surface engineering design of Al2O3/Mo self-lubricating structural ceramics - Part II: Continuous lubrication effects of a three-dimensional lubricating layer at temperatures from 25 to 800 degrees C 期刊论文
Wear, 2016, 卷号: 360-361, 页码: 97-103
Authors:  Fang Y(方媛);  Fan HZ(樊恒中);  Song JJ(宋俊杰);  Zhang YS(张永胜);  Hu LT(胡丽天);  Zhang YS(张永胜)
Adobe PDF(2843Kb)  |  Favorite  |  View/Download:188/2  |  Submit date:2016/08/24
Ceramic-matrix Composite  Laser Processing  High Temperature  Sliding Wear  Tribochemistry  Solid Lubricants  
Surface composition-lubrication design of Al2O3/Mo laminated composites—Part I: Influence of laser surface texturing on the tribological behavior at 25 and 800 °C 期刊论文
Wear, 2015, 卷号: 334, 页码: 23-34
Authors:  Fang Y(方媛);  Zhang YS(张永胜);  Fan HZ(樊恒中);  Hu TC(胡天昌);  Song JJ(宋俊杰);  Hu LT(胡丽天);  张永胜
Adobe PDF(7207Kb)  |  Favorite  |  View/Download:162/1  |  Submit date:2015/10/29
Ceramic-matrix Composite  Laser Processing  High Temperature  Sliding Wear  Tribochemistry  Solid Lubricants  
Preparation, microstructure and tribological behavior of laser cladding NiAl intermetallic compound coatings 期刊论文
Wear, 2012, 卷号: 274, 页码: 298-305
Authors:  Yu YJ(俞友军);  Zhou JS(周健松);  Chen JM(陈建敏);  Zhou HD(周惠娣);  Guo C(郭纯);  Wang LQ(王凌倩);  Yang LB(杨连斌);  Chen JM(陈建敏)
Adobe PDF(2025Kb)  |  Favorite  |  View/Download:270/4  |  Submit date:2013/07/12
Nial Coating  Intermetallics  Laser Processing  Wear Testing  
High temperature wear resistance of laser cladding NiCrBSi and NiCrBSi/WC-Ni composite coatings 期刊论文
Wear, 2011, 卷号: 270, 页码: 492-498
Authors:  Guo C(郭纯);  Zhou JS(周健松);  Chen JM(陈建敏);  Zhao JR(赵杰荣);  Zhou HD(周惠娣)
Adobe PDF(2177Kb)  |  Favorite  |  View/Download:294/4  |  Submit date:2012/09/24
Metal–matrix Composite  Laser Processing  High Temperature  Sliding Wear