Accelerated degradation of polyetheretherketone and its composites in the deep sea | |
Department | 固体润滑国家重点实验室 |
Liu H(刘昊); Wang JZ(王建章); Jiang PF(姜朋飞); Yan FY(阎逢元) | |
2018-07-23 | |
Source Publication | Royal Society Open Science |
Volume | 5Issue:1Pages:171775 |
Keyword | Degradation Polyetheretherketone Composites Deep Sea Hydrostatic Pressure |
DOI | 10.1098/rsos.171775 |
URL | 查看原文 |
If | 2.642 |
Language | 英语 |
compositor | 第一作者单位 |
Citation statistics | |
Document Type | 期刊论文 |
Identifier | http://ir.licp.cn/handle/362003/24282 |
Collection | 固体润滑国家重点实验室(LSL) |
Corresponding Author | Wang JZ(王建章); Yan FY(阎逢元) |
Recommended Citation GB/T 7714 | Liu H,Wang JZ,Jiang PF,et al. Accelerated degradation of polyetheretherketone and its composites in the deep sea[J]. Royal Society Open Science,2018,5(1):171775. |
APA | Liu H,Wang JZ,Jiang PF,&Yan FY.(2018).Accelerated degradation of polyetheretherketone and its composites in the deep sea.Royal Society Open Science,5(1),171775. |
MLA | Liu H,et al."Accelerated degradation of polyetheretherketone and its composites in the deep sea".Royal Society Open Science 5.1(2018):171775. |
Files in This Item: | There are no files associated with this item. |
Items in the repository are protected by copyright, with all rights reserved, unless otherwise indicated.
Edit Comment